MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurotec® Tecodur® PB70 GR30 NL100 IL PBT, 30% glass fiber reinforced, impact modified, natural
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Impact Grade

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183
Moisture Absorption 0.100 %
@Temperature 23.0 °C
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0030 cm/cmEurotec
Linear Mold Shrinkage, Transverse 0.011 cm/cmEurotec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPaISO 527
Elongation at Break 3.5 %ISO 527
Tensile Modulus 8500 MPaISO 527
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 195 °CISO 75
Flammability, UL94 HB
@Thickness 0.750 mm
 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 270 °C
Feed Temperature 50.0 - 70.0 °CThroat
Mold Temperature 60.0 - 100 °C
Drying Temperature 120 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.080 %ISO 960
Hold Pressure 40.0 - 80.0 MPa
 
Descriptive Properties
Back PressureLow
Injection SpeedFast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Edinburg Plastics BTA706 PBT, Impact Modified
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT
Celanese Crastin® HR5330HFS NC010 PBT-IGF30
BLUESTAR 403G-MG30 PBT, 30% Glass Filled
RTP Company RTP 1000 HI Polybutylene Terephthalate (PBT) Impact Modified

PEUROS108 / 147098

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.