MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Industeel TENASTEEL® Cold Work Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: Description: TENASTEEL is a cold work tool steel, combining a high wear resistance together with a very high toughness. Its other advantages are a good machinability in the as-delivery condition and a particularly high resistance to thermal softening. The steel is delivered in the soft annealed condition with a maximum hardness of 250 HB. TENASTEEL is specially designed to replace D2 type steels widely used by toolmakers but suffering from an excessive brittleness. Thanks to its chemistry increasing resistance to softening during tempering, TENASTEEL is especially suited for all processes of surface treatment and coatings commonly used in the market, including nitriding processes involving high temperatures.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 250<= 250Typical in annealed condition
Hardness, Rockwell C 6060Heat Treated
Modulus of Elasticity 205 GPa29700 ksiTypical
Compressive Strength 2300 MPa334000 psiTypical
Charpy Impact, Unnotched 25.0 J18.4 ft-lbTypical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.2 µm/m-°C
@Temperature 20.0 - 100 °C
5.67 µin/in-°F
@Temperature 68.0 - 212 °F
 11.3 µm/m-°C
@Temperature 20.0 - 200 °C
6.28 µin/in-°F
@Temperature 68.0 - 392 °F
 11.9 µm/m-°C
@Temperature 20.0 - 300 °C
6.61 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 21.0 W/m-K
@Temperature 20.0 °C
146 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.0 %1.0 %
Chromium, Cr 7.5 %7.5 %
Iron, Fe 88.245 - 88.25 %88.245 - 88.25 %As remainder
Manganese, Mn 0.35 %0.35 %
Molybdenum, Mo 2.6 %2.6 %
Sulfur, S <= 0.0050 %<= 0.0050 %
Vanadium, V 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Assab Steels ASSAB XW-41 Cold Work Steel
Assab Steels ASSAB XW-5 Cold Work Steel
Assab Steels ASSAB XW-42 Cold Work Steel
Overview of materials for High Carbon Steel
Oboto Wood

NINDUST54 / 17592

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.