MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis TD315BF Polypropylene Terpolymer
Categories: Polymer

Material Notes: TD315BF is a C2/C4 terpolymer. This grade is designed for sealing layers of oriented and non oriented films. CAS-No. 25895-47-0
TD315BF contains:
Antiblocking agent: 1000 ppm
Slip agent: 1000 ppm
Calcium stearate: yes

Typical characteristics:

  • Lowest volatiles and fumes during processing High seal strength and hot tack force
  • Low content of amorphous polymer High sealing window
  • Low taste & odor Excellent optical properties
  • Excellent printability Optimized balance between high melting point for easy
  • Good stability of surface tension Processing and low sealing temperature
Applications:
  • Sealing layer in coextrusion
  • Food packaging film
  • Lamination film
Additives: TD312BF contains antiblock but no slip agent

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 6.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.700 GPa102 ksiISO 178
Heat Seal Strength Initiation Temperature 105 °C221 °FMeasured on 50 µm film.
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °F
Vicat Softening Point 115 °C
@Load 1.02 kg
239 °F
@Load 2.25 lb
ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9920 / 323277

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.