Resin Type: Homopolymer Characteristics: Excellent Clarity, Good Impact Strength, Excellent Processability, Low Coefficient of Friction, Good Sealability Applications:Bread Bag, Dry Goods Packaging, Produce and Hardware Packaging Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1. Film properties below based on film thickness of 31.8 µm. Data provided by Chevron Chemical. |