MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parker Chomerics Tecknit Teckfip™ FIP-A Formed in Place Conductive Elastomer
Categories: Polymer

Material Notes: Description: This compound is ideally suited to corrosion-concerned applications where the gasket is applied to an aluminum casting. The corrosion resistance is enhanced due to the galvanic compatibility between the casting and the conductive Aluminum/Copper particle used. The compression set performance is good and this compound offers a very stable EMI shielding performance even under large mechanical stress. The electrical conductivity performance and EMI shielding is very similar to the high performing FIP-C elastomer gasket.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.975 - 4.025 g/cc2.975 - 4.025 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 57 - 6757 - 67
Tensile Strength >= 0.621 MPa>= 90.0 psi
Elongation at Break >= 30 %>= 30 %
Peel Strength >= 9.00 kN/m>= 51.4 pli
Compression Set 15 - 25 %15 - 25 %
 15 %
@Temperature 70.0 °C,
Time 79200 sec
15 %
@Temperature 158 °F,
Time 22.0 hour
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.010 ohm-cm<= 0.010 ohm-cm
Surface Resistance <= 0.020 ohm<= 0.020 ohm
 <= 0.020 ohm
@Temperature 85.0 °C,
Time 605000 sec
<= 0.020 ohm
@Temperature 185 °F,
Time 168 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour
Tack-Free Time 12.0 min0.200 hour
Shelf Life 1.00 Month1.00 MonthSyringe
 6.00 Month6.00 MonthCartridge
 
Descriptive Properties
ColorSilver/Tan
FillerSilver Aluminum Heat Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME363 / 131073

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.