MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Vinnapas® SAF 34 Styrene/Acrylate Copolymer
Categories: Polymer; Thermoplastic

Material Notes: Product description: VINNAPAS® SAF 34 is a fine-particle dispersion of a special styrene/acrylate copolymer. It is free from alkyl phenol ethoxylate (APEO) containing compounds.

Application: VINNAPAS® SAF 34 has an excellent pigment-binding capacity and very good adhesion to inorganic substrates. VINNAPAS® SAF 34 has proved for many years to be an outstanding binder in many fields of application and versatility is its special strength. VINNAPAS® SAF 34 is a high performance binder for interior and exterior paints, dispersion modified silicate paints and plasters, silicone paints and plasters, synthetic resin bound plasters and roof coatings. VINNAPAS® SAF 34 is an ideal binder for manufacturing construction and tile adhesive paste with extremely good wet adhesion properties. Films produced from this dispersion have an excellent resistance to water and alkalis, with only slight water absorption and greatly delayed whitening. Paints and plasters based on this dispersion therefore show very little tendency to soften under prolonged immersion in water. VINNAPAS® SAF 34 is an outstanding binder for exterior masonry paints which show very low dirt pickup. Conventional masonry paints are frequently formulated below the critical pigment volume concentration (CPVC) but silicone resin paints must be permeable to water vapor and therefore should be formulated above the CPVC. WACKER silicone masonry water repellants like SILRES® BS 45 and SILRES BS® 1306 show good compatibility with VINNAPAS® SAF 34 and silicone resin paints containing VINNAPAS® SAF 34 exhibit excellent water repellency and low capillary water absorption. If VINNAPAS® SAF 34 is to be used in dispersion silicate paints, the compatibility with the corresponding water glass should always be checked. VINNAPAS® SAF 34 is particularly recommended for producing pasty construction adhesives, which must have outstanding strength even when exposed to water. This improved wet adhesion is particularly useful for ceramic tiles adhesives.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³DIN EN ISO 2811-1
Solids Content 49 - 51 %49 - 51 %DIN EN ISO 3251
Particle Size 100 µm100 µm
pH 7.5 - 8.57.5 - 8.5DIN/ISO 976
Brookfield Viscosity 6000 - 12000 cP6000 - 12000 cPspindle 5/20 rpm; DIN EN ISO 2555
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiDIN EN ISO 527-3
Elongation at Break 600 %600 %DIN EN ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 20.0 °C68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Vinnol® E 15/40 A TF Vinyl Chloride Copolymer
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Inovyn 460SL Polyvinyl Chloride grafted copolymer

PWACK9654 / 205183

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.