MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES Luriblend® PA6/6 GF30 TL15 UV 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized; Nylon 66, PTFE Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Heat Stabilizer, UV Stabilizer and PTFE Lubricant(15%)

Features: Lubricated, Good Wear Resistance, Low Friction, Good UV Resistance and Heat Stabilized

Appearance: Natural Color

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccASTM D792
Water Absorption 0.50 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D785
Tensile Strength, Yield 21600 psiASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Strength 32500 psiASTM D790
Flexural Modulus 1.30e+6 psiASTM D790
Izod Impact, Notched 1.40 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Coefficient of Friction, Dynamic 0.28ASTM D1894
Coefficient of Friction, Static 0.22ASTM D1894
K (wear) Factor 18.0 x 10-10 in³-min/ft-lb-hr
Limiting Pressure Velocity 17500 psi-ft/min10 fpm
 17500 psi-ft/min1000 fpm
 20000 psi-ft/min100 fpm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 500 V/milMethod A (Short-Time); ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 498 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 490 °FUnannealed; ASTM D648
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 205 TFE 15 UV Nylon 6/6 (PA), Glass Fiber - PTFE Lubricated - UV Stabilized
Avient LubriOne™ ATH-000/04S Acetal (POM) Homopolymer
Lehvoss LUVOTECH® GS 58 Polyamide 66 with glass fiber, lubricant modified
Lehvoss LUVOTECH® 1-9513 Polyamide 66 with glass fiber, PTFE, lubricant modified, heat stabilized
Lehvoss LUVOCOM® 1-1129 Polyamide 66 with glass fiber, PTFE, lubricant modified, heat stabilized

PTPC0827 / 136765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.