MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Alliance BCN-15 Bonded (Composite) Magnetic Material  (discontinued **)
Categories: Ceramic; Metal; Electronic/Magnetic Alloy

Key Words: Magnet Magnets
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 5.60 - 6.00 g/cc0.202 - 0.217 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 37.0 MPa5370 psi
Modulus of Elasticity 0.700 - 1.00 GPa102 - 145 ksi
Compressive Strength 80.0 - 120 MPa11600 - 17400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00100 - 0.00300 ohm-cm0.00100 - 0.00300 ohm-cm
Magnetic Coercive Force, Hc 5500 Oe5500 Oe
 12500 Oe12500 OeIntrinsic
Magnetic Remanence, Br 6300 Gauss6300 Gauss
Magnetic Maximum Energy Product, BH 8.7 MGOe8.7 MGOe
Curie Temperature 300 - 470 °C572 - 878 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 30.0 µm/m-°C
@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F
@Temperature 68.0 °F
Parallel DOM
Specific Heat Capacity 0.400 J/g-°C0.0956 BTU/lb-°F
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 160 °C320 °F
 
Descriptive Properties
Reversible Temp Coef., Bd-0.14 %/°C
Reversible Temp Coef., Hd-0.36 %/°C
Temperature Coefficient, Br-0.11 %/°C(20-100°C)
Temperature Coefficient, Hci-0.39 %/°C(20-100°C)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance S-28B Samarium Cobalt Magnetic Material
Alliance S-30A Samarium Cobalt Magnetic Material
Alliance BCN-10 Bonded (Composite) Magnetic Material
Alliance BCN-13 Bonded (Composite) Magnetic Material
Alliance BCN-12 Bonded (Composite) Magnetic Material

NALLIAN69 / 14894

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.