MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kohesi Bond KB 1427 HT One component, chemically resistant epoxy for bonding, coating, sealing and casting
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Highlights:
  • service up to 340°C
  • Admirable chemical resistance
  • Excellent flow properties
  • Low exotherm upon curing
  • Superior electrical insulation
  • Unlimited working life at room temperature
Kohesi Bond KB 1427 HT is a marvelous single component epoxy system for bonding, coating, sealing and casting applications. Although it requires a minimum temperature of 150°C for curing, it can achieve faster cures at elevated temperatures. KB 1427 HT offers an extremely wide service temperature range of -60°C to +340°C, with a roaring glass transition temperature (Tg) of 220°C - 230°C. This product’s exquisite flow properties and unlikely low exotherm makes it ideal for use in casting well beyond 1/2 inch thicknesses. Being a one component system, it provides ease of application and also adheres well to a wide variety of substrates including metals, ceramics, composites, most plastics and glass. It provides first-rate mechanical strength properties and dimensional stability. In addition to superior electrical insulation, KB 1427 HT also offers excellent chemical resistance to a variety of fuels, oils and water even at higher temperatures. It has a tan color. It is highly recommended to post cure the epoxy at 180°C for 2 - 12 hours in order to achieve optimum properties. Owing to its magnificent performance and ease of use, KB 1427 HT is ideal for use in aerospace, oil and chemical processing, electronics and various OEM applications.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Casting

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 15000 - 24000 cP15000 - 24000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Modulus 2.90 - 3.10 GPa420 - 450 ksi
Compressive Strength >= 145 MPa>= 21000 psi
Adhesive Bond Strength  >= 15.2 MPa
@Temperature 200 °C
>= 2200 psi
@Temperature 392 °F
Tensile Lap Shear, Al/Al
 >= 22.8 MPa
@Temperature 23.0 °C
>= 3300 psi
@Temperature 73.4 °F
Tensile Lap Shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dissipation Factor 0.0080
@Frequency 60 Hz
0.0080
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 340 °C644 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 220 - 230 °C428 - 446 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  240 - 360 min
@Temperature 180 °C
4.00 - 6.00 hour
@Temperature 356 °F
Option 2
 300 - 360 min
@Temperature 150 °C
5.00 - 6.00 hour
@Temperature 302 °F
Option 1
 960 - 1800 min
@Temperature 150 - 180 °C
16.0 - 30.0 hour
@Temperature 302 - 356 °F
Optimum Cure: 150°C for 4 - 6 hours, plus 180°C for 12 - 24 hours
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 Monthin original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOHESI939 / 249118

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.