Description: RHEOCIN T is processed castor oil derivatives that are use for rheological modification of non-aqueous systems. Application: RHEOCIN T is a thixothrope for aliphatic systems - Trade sales alkyds
- Industrial alkyds
- Stains
- Other aliphatic coating systems
Information provided by Southern Clay Products |