Vyncolit® BXE650/1 is an inorganic filled phenolic molding compound with excellent isotropic properties, superior dimensional stability and very high mechanical properties, even at elevated temperatures.Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |