MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Epoxy Technology EPO-TEK® OG159-2 UV Cure Optical Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Material Description: A single component, high viscosity, UV curable epoxy adhesive designed for sealing glass plates together in the LCD/OLED/display industry. It contains 1mil glass beads for bond line control. Common applications include semiconductor, electro-optics, fiber optic, and scientific/OEM. It can be applied by screen printing or dispensing techniques. It is capable of coating, adhering, sealing, and encapsulating devices.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/cc
Particle Size <= 30 µm<= 30 µm
Viscosity 100000 - 140000 cP
@Temperature 23.0 °C
100000 - 140000 cP
@Temperature 73.4 °F
2.5 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969
Tensile Modulus 2.35 GPa341 ksiStorage
Shear Strength >= 11.7 MPa>= 1700 psiDie
 
Thermal PropertiesMetricEnglishComments
CTE, linear 58.0 µm/m-°C32.2 µin/in-°FBelow Tg
 240 µm/m-°C133 µin/in-°FAbove Tg
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 30.0 °C>= 86.0 °FPost-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min
Decomposition Temperature 443 °C829 °FDegradation Temperature
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5679
@Wavelength 589 nm
1.5679
@Wavelength 589 nm
Transmission, Visible  >= 90 %
@Wavelength 400 nm
>= 90 %
@Wavelength 400 nm
Spectral
 >= 98 %
@Wavelength 580 - 2000 nm
>= 98 %
@Wavelength 580 - 2000 nm
Spectral
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorWhitebefore cure
ConsistencyThixotropic paste
Number of ComponentsSingle
Weight Loss0.13%200°C
 0.44%250°C
 0.97%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA A430 LCP, 25% Specialty
AISI Type P20 Mold Steel (UNS T51620)
Epoxy Technology EPO-TEK® OG198-54 UV Cure Optical Epoxy

PPOXYT168 / 141207

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.