MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ASTM D2240
Tensile Strength, Yield 46.9 MPa6800 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.76 GPa400 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 95.1 MPa13800 psiASTM D790
Flexural Modulus 3.10 GPa450 ksiASTM D790
Izod Impact, Notched 11.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
Dart Drop Total Energy  57.8 J/cm
@Temperature 23.0 °C
0.108 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 200 J/cm
@Temperature 23.0 °C
0.375 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 63.0 µm/m-°C35.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
@Thickness 3.18 mm
165 °F
@Thickness 0.125 in
Compression Molded, Annealed at 50 deg.C; ASTM D648
Flammability, UL94 V-0V-0UL 94
 5VA5VAUL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 - 204 °C376 - 399 °F
 
Descriptive Properties
Agency RatingsNSF 51The E6950 natural 0000 is the only NSF 51 listed color in this product.
FeaturesMedium Impact Resistance
FormsPowder
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification1-41443-33-0000ASTM D4216
 16354ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Rigid Grade
Overview of materials for PVC, Molded
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Geon® Performance Solutions Vinyl Rigid Extrusion 87262 Polyvinyl Chloride, Rigid

PH0POL0233 / 144802

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.