MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Estane® BCXA07 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Polyether Thermoplastic Polyurethane (TPU)

Features: Excellent foam-ability, superior rebound resiliency, compression set and low temperature properties

Uses: Foam injection molding and extrusion foaming. Preliminary data.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.300 g/cc0.300 g/ccFoam Injection Molded Part; ASTM D-792
 1.06 g/cc1.06 g/ccASTM D-792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 79
@Time 5.00 sec
79
@Time 0.00139 hour
ASTM D-2240
Tensile Strength 25.0 MPa3630 psiASTM D-412
Elongation at Break 750 %750 %ASTM D-412
Compression Set 4.0 %4.0 %50,000 cycles
 5.0 %
@Temperature 23.0 °C
5.0 %
@Temperature 73.4 °F
ASTM D-395
 11 %
@Temperature 50.0 °C
11 %
@Temperature 122 °F
ASTM D-395
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °F
Glass Transition Temp, Tg -66.0 °C-86.8 °F
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 204 °C399 °F
Zone 1 182 °C360 °F
Zone 2 193 °C379 °F
Zone 3 204 °C399 °F
Zone 4 204 °C399 °F
Mold Temperature 35.0 - 49.0 °C95.0 - 120 °F
Drying Temperature 104 °C
@Time 7200 - 14400 sec
219 °F
@Time 2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Energy Efficiency0.21Change after 50,000 cycles
 0.42Initial
Foam Hardness32Asker C, ASTM D-2240
Foam Vertical Resiliency0.58ASTM D-2632

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding
Lubrizol LifeSciences Tecoflex® EG-85A TPU - Clear
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlbond® 580 Thermoplastic Polyurethane

PLUBR5001 / 238871

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.