MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Tabriz HD 6040 UA High Density Polyethylene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: HD6040UA is high density polyethylene copolymer containing butene-1(C4) as comonomer with medium content of light stabilizer additive HD6040UA has good impact strength, excellent surface finish. Applications: large dustbins and pails, pallet.

Information provided by Tabriz Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D1505
Brightness 60.0 %Whiteness Index; ASTM E313
Melt Flow 3.7 g/10 min
@Load 2.16 kg
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPaASTM D638
Elongation at Break 700 %ASTM D638
Charpy Impact, Notched 10.0 kJ/m²ASTM D6110
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 112 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Yellow Index -1.00 %ASTM E313
 
Descriptive Properties
Contamination (No.)5BP137

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTABRZ904 / 198215

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.