MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Unifrax Fiberfrax® 882-H Ceramic Fiber Paper
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: This product is completely free of organics and used when higher fired strength is required or in processes and applications where even small amounts of organic burnout is unacceptable. 882-H has higher temperature stability and higher density than 972-H paper. The fiber geometry and product density lead to the maximum burn strength of an unbindered paper.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.256 g/cc0.00926 lb/in³
Loss On Ignition 0.10 %0.10 %including binder
 
Thermal PropertiesMetricEnglishComments
Melting Point 1927 °C3501 °F
Maximum Service Temperature, Air 1150 °C2100 °FRecommended Operating Temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 58 - 60 %58 - 60 %
Fe2O3 <= 0.10 %<= 0.10 %
SiO2 40 - 42 %40 - 42 %
 
Descriptive Properties
ColorWhite
Fiber Index (% Wt)45
Na2O3 (%)<0.3
Temperature Grade (°C)1427

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® HP-S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator

CUNIF009 / 97781

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.