MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound  (discontinued **)
Categories: Ceramic; Polymer; Thermoset; Epoxy

Material Notes: Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a thickness of 3 mm (1/8”) or more. Non-shrinking. 100% Solids. ARC MX5 is formulated with a high concentration of small ceramic beads and particles for extremely abrasive environments where metal loss is often repaired by more conventional and costly weld overlay. ARC MX5 can be used either to rebuild eroded metal surfaces or to provide a wear resistant, sacrificial surface which frequently outperforms the original metal, rubber liners, ceramic tiles or weld overlay. ARC MX5 is chosen over other ARC Composites for abrasion when a rapid cure, emergency repair is needed.

Benefits:

  • Excellent wear characteristics of ARC MX5 extend equipment operating cycles.
  • Tough resin structures resist thermal-mechanical shock
  • Outstanding adhesion results in reliable performance with no undercutting
  • Ease of application reduces labor and downtime costs
  • Rapid cure allow return to service in 1 hour or less.
  • Easily shaped and formed to any metal surface.

Suggested Uses:

  • Pneumatic Conveyors
  • Chipper and Chip Bins
  • Hydro Pulpers
  • Turbo Separators
  • Ni-Hard Slurry Pumps
  • Fly Ash Separators
  • Wood Chip Transport Fans
  • Screw Conveyors
  • Exhaust Fans
  • Cyclones, Hoppers
  • Wear Plates
  • Pipe Elbows
  • Pulverized Fuel Lines
  • Pulverizers

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.20 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89ASTM D2240
Tensile Strength at Break 2400 psiASTM D638
Flexural Strength 3500 psiASTM D790
Compressive Strength 9200 psiASTM D695
Impact Test 58.0 in-lbReverse; ASTM D2794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 60.0 °CWet Service
 120 °CDry Service
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 hour
@Temperature 43.0 °C
Light Load
 0.330 hour
@Temperature 32.0 °C
Light Load
 0.500 hour
@Temperature 25.0 °C
Light Load
 0.500 hour
@Temperature 43.0 °C
Full Load
 0.750 hour
@Temperature 32.0 °C
Full Load
 1.00 hour
@Temperature 16.0 °C
Light Load
 1.00 hour
@Temperature 25.0 °C
Full Load
 2.00 hour
@Temperature 10.0 °C
Light Load
 2.00 hour
@Temperature 16.0 °C
Full Load
 4.00 hour
@Temperature 10.0 °C
Full Load
 12.0 hour
@Temperature 43.0 °C
Full Chemical
 18.0 hour
@Temperature 32.0 °C
Full Chemical
 24.0 hour
@Temperature 25.0 °C
Full Chemical
 36.0 hour
@Temperature 16.0 °C
Full Chemical
 48.0 hour
@Temperature 10.0 °C
Full Chemical
Tack-Free Time 0.0830 hour
@Temperature 43.0 °C
 0.167 hour
@Temperature 32.0 °C
 0.250 hour
@Temperature 25.0 °C
 0.4167 hour
@Temperature 16.0 °C
 0.583 hour
@Temperature 10.0 °C
 
Descriptive Properties
ColorGray

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTCHS028 / 138140

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.