MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Estane® ZHF 82AT3 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Estane® ZHF 82AT3 is 82A aromatic Polyether-Based, Non-Halogen Flame Retardant, Thermoplastic Polyurethane (TPU) Compound

Features: Soft, Matte finished, Non-Halogen flame retardant

Uses: Wire and cable and general extrusion where flame retardant properties are required

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccISO 2781
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 80 - 84
@Time 5.00 sec
80 - 84
@Time 0.00139 hour
ISO 868
Tensile Strength 24.5 MPa3550 psiISO 527
Elongation at Break 620 %620 %ISO 527
100% Modulus 4.90 MPa
@Strain 100 %
711 psi
@Strain 100 %
ISO 527
300% Modulus 8.20 MPa
@Strain 300 %
1190 psi
@Strain 300 %
ISO 527
Tear Strength 50.1 kN/m286 pliDie C, Nicked; ISO 34-1B
 101.1 kN/m576.9 pliDie C, Un-nicked; ISO 34-1B
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-2V-2
 
Processing PropertiesMetricEnglishComments
Zone 1 160 °C320 °F
Zone 2 170 °C338 °F
Zone 3 175 °C347 °F
Zone 4 180 °C356 °F
Adapter Temperature 180 °C356 °F
Die Temperature 170 °C338 °Fzone 2
 175 °C347 °Fzone 1
Drying Temperature 105 °C
@Time 10800 sec
221 °F
@Time 3.00 hour
Dew Point -40.0 °C-40.0 °Fpreferable
 <= -30.0 °C<= -22.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® ZHF 78AT3 Thermoplastic Polyurethane

PLUBR5003 / 238873

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.