MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker HDK® H13L Silica
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Synthetic, hydrophobic, amorphous silica, produced via flame hydrolysis.

Special features: White colloidal powder of high purity.

Application: HDK® H13L is applied as a thickening, thixotropic and antisedimentation agent in coatings, printing inks, adhesives and others. It is mainly used in polar systems. Due to its strong hydrophobicity HDK® H13L is well suited for solvent free systems, for high solids and for waterborne coatings.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.0500 - 0.0850 g/cc0.00181 - 0.00307 lb/in³tamped; DIN EN ISO 787-11
Density 2.20 g/cc0.0795 lb/in³DIN 51757
pH 3.8 - 4.83.8 - 4.84% dispersion; DIN EN ISO 787-9
Specific Surface Area 100 m²/g100 m²/gHydrophobic Silica
 110 - 140 m²/g110 - 140 m²/gHydrophobic Silica
Evaporation Loss <= 0.060 %
@Temperature 105 °C,
Time 7200 sec
<= 0.060 %
@Temperature 221 °F,
Time 2.00 hour
DIN EN ISO 787-2
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.60 - 2.2 %0.60 - 2.2 %DIN ISO 10694
SiO2 >= 99.8 %>= 99.8 %based on the substance heated at 1000°C for 2 h; DIN EN ISO 3262-19
 
Descriptive Properties
Content (%)50Residual silanol
Sieve residue<0.05%acc to Mocker >40 µm, DIN EN ISO 787-18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Wacker® TES 28 Silicate
Wacker Belsil® DM 3112 VP Dimethiconol - Emulsion

PWACK9340 / 204869

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.