MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Danquinsa DANTHANE® 126KB-Powder TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: DANTHANE_ 126KB-Powder is a polyester based aromatic TPU, already colored in blue. This TPU-powder is suitable for sinter coating, mainly at the production of technical textiles. It can be reached medium-hard surface coatings, like they will be needed for example for the production of transport and conveyer belts, flat belt materials, flexible containers and textile lining materials. DANTHANE_ 126KB-Powder can be used as intermediate layer and top coat. Very often DANTHANE_ 126KB-Powder is used as intermediate layer and then, as top coat, the transparent type DANTHANE_ 126K-Powder is used.

Application: DANTHANE_ 126KB-Powder is applied at the hot melt coating of industrial textiles. The coated textiles are used for transport and drive sections. This TPU-powder, colored in blue, can be used at the coating as intermediate layer and top coat. Very often DANTHANE_ 126KB-Powder is used as intermediate layer and than, as top coat, the transparent type DANTHANE_ 126K-Powder is used. For the coating of textiles we also deliver the corresponding impregnations and primers with the DANCOLL_ products.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDIN 53.479
Particle Size 50 - 500 µmPowder grit size
Melt Flow 65 - 95 g/10 min
@Load 10.0 kg,
Temperature 190 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94DIN 53.505
Hardness, Shore D 36DIN 53.505
Tensile Strength 35.0 MPaDIN 53.504
 25.0 - 30.0 MPa
@Temperature 80.0 °C,
Time 1.81e+6 sec
Immersion in water; DIN 53.504
Elongation at Break 420 %DIN 53.504
 450 - 530 %
@Temperature 80.0 °C,
Time 1.81e+6 sec
Immersion in water; DIN 53.504
Tensile Modulus 5.00 MPa
@Strain 20 %
DIN 53.504
100% Modulus 13.0 MPaDIN 53.504
300% Modulus 15.0 MPaDIN 53.504
Resilience 37[%]; DIN 53.512
Tear Strength 90.0 kN/mpropagation resistance; DIN 53.515
Abrasion 30[mm³]; DIN 53.516
Compression Set 25 %
@Temperature 23.0 °C,
Time 252000 sec
DIN 53.517
 60 %
@Temperature 70.0 °C,
Time 86400 sec
DIN 53.517
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 - 175 °CKofler
Softening Point 140 - 160 °CKofler
Glass Transition Temp, Tg -22.0 °CDSC; DIN 51.007
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %
Shelf Life 6.00 Month
 
Descriptive Properties
AspectBlue colored powdercolor RAL 5015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ151 / 294571

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.