MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel; Tool Steel; Hot Work Steel

Material Notes: Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and temper resistance, along with moderate wear resistance. It is air hardenable and is used in most applications in the heat treated condition at HRC 44-52. The normal tempering temperatures for Nu-Die V are quite high (>1000°F, 540°C), allowing it to retain its heat treated hardness and strength while in service at elevated temperatures. Nu-Die V may be used for tool temperatures up to about 1000°F (540°C) with brief exposures up to 1100°F (595°C), making it ideal for forging dies, hot extrusion tooling, and die casting dies. Crucible offers two premium versions, Nu-Die XL and Nu-Die ESR, for applications requiring critical polishability, improved heat check resistance and better transverse toughness.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 192 - 235192 - 235Annealed
Hardness, Rockwell C 40 - 4240 - 42Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C
 51 - 5351 - 53Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C
Modulus of Elasticity 207 GPa30000 ksi
Charpy Impact 14.0 J10.3 ft-lbAustenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C
 24.0 J17.7 ft-lbAustenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 20.0 - 95.0 °C
6.11 µin/in-°F
@Temperature 68.0 - 203 °F
 11.5 µm/m-°C
@Temperature 20.0 - 205 °C
6.39 µin/in-°F
@Temperature 68.0 - 401 °F
 12.6 µm/m-°C
@Temperature 20.0 - 540 °C
7.00 µin/in-°F
@Temperature 68.0 - 1000 °F
Thermal Conductivity  26.0 W/m-K
@Temperature 95.0 °C
180 BTU-in/hr-ft²-°F
@Temperature 203 °F
 27.7 W/m-K
@Temperature 315 °C
192 BTU-in/hr-ft²-°F
@Temperature 599 °F
Shrinkage -0.0600 %
@Treatment Temp. 540 - 620 °C
-0.0600 %
@Treatment Temp. 1000 - 1150 °F
Tempered 540-620°C
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.40 %0.40 %
Chromium, Cr 5.2 %5.2 %
Iron, Fe 91.15 %91.15 %As Remainder
Molybdenum, Mo 1.3 %1.3 %
Silicon, Si 1.0 %1.0 %
Vanadium, V 0.95 %0.95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
Bohler-Uddeholm SUPERIOR® H13 Hot Work Tool Steel
AISI Type H13 Hot Work Tool Steel
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel

NCRUC017 / 16010

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.