MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LG Chemical LUPOY GP-5000FQ General Purpose PC/ABS Alloy, Unreinforced, Excellent Flow  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.

Applications:

    Automotive: Automotive front ends, cluster pad main panel (instrument panel), lower cluster pad main, console box, glove box cover, door, wheel cover and cap, defroster grill, back mirror housing

    Electrical and Electronic: Monitor housing, fax housing, notebook PC housing, cellular phone case, fax and copy machine frame, CD ROM drive tray and main frame, relay case, connector, switch

    Industrial Parts and Household Appliance: Helmet, terminal box, electrical tool housing, industrial bobbin, distributing board box, power tool component, gears and cams, water meter housing

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D792
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 250 °C
14 g/10 min
@Load 4.76 lb,
Temperature 482 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
Tensile Strength, Yield 56.0 MPa8120 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Flexural Strength 82.0 MPa11900 psiASTM D790
Flexural Modulus 2.40 GPa348 ksiASTM D790
Izod Impact, Notched 2.95 J/cm
@Temperature 23.0 °C
5.53 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °FASTM D648
Flammability, UL94 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 270 °C446 - 518 °F
Middle Barrel Temperature 240 - 280 °C464 - 536 °F
Front Barrel Temperature 250 - 290 °C482 - 554 °F
Nozzle Temperature 250 - 290 °C482 - 554 °F
Melt Temperature 260 - 300 °C500 - 572 °F
Mold Temperature 70.0 - 110 °C158 - 230 °F
Drying Temperature 70.0 - 100 °C158 - 212 °F
Dry Time 3 - 5 hour3 - 5 hour
Screw Speed 40 - 70 rpm40 - 70 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy
LG Chemical LUPOY GP-5306F General Purpose PC/ABS Alloy, 30% Polymer Alloy, Weather Resistant, Flame Retardant
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength

PLGCHEM054 / 50875

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.