MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Tixogel® VP-V Organoclay
Categories: Ceramic; Clay

Material Notes: Description: Tixogel® VP-V is a vegetable derived Organoclay Thixotrope designed for use in cosmetic and personal care systems to develop thixotropic rheological control. It is designed to impart a high degree of gelling efficiency over a wide range of low to medium polarity fluids

Application:

  • Skin cleansers Lip products
  • Sun skincare products Creams
  • Lotions Makeup.
  • Suitable Solvents
  • Volatile Silicone Fluids Mineral Spirits
  • Vegetable Oil Mineral Oils

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 3.0 %
 
Descriptive Properties
Bulking Value0.0667 US gallons/pound
Color/FormLight cream powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Tixogel® TE Organoclay Additive
BYK Tixogel® Y-25XP Additive
BYK Tixogel® MP 100 V Organoclay
BYK Tixogel® MPG Organoclay
BYK Tixogel® MPI Organoclay

PBYK123 / 185120

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.