Product Description: Master Bond Polymer System EP21SC-1 is a two component epoxy system featuring abrasion resistance. This high performance compound utilizes silicon carbide as a filler material and can be used as a coating, adhesive or sealant. It has a convenient, non-critical one to one mix ratio by weight or volume. It is 100% reactive and does not contain any solvents or diluents. Also, the system has minimal shrinkage upon cure. Not only does EP21SC-1 offer good abrasion resistance, it can also withstand exposure to chemicals including water, oils, hydraulic fluids, acids and bases over the wide temperature range of -60°F to 250°F. It has very good adhesion to treated metals, ceramics and many plastics. EP21SC-1 cures rigid with a Shore D over 95. It has good electrical insulation properties and its thermal expansion coefficient is desirably low. The color of Parts A and B is dark gray. EP21SC-1 is widely used in chemical and mechanical processing, maintenance and tank and chute applications, where excellent abrasion resistance is needed. Product Advantages: - Convenient mixing: non-critical one to one weight or volume mix ratio.
- Easy application: smooth paste consistency.
- Versatile cure schedules: convenient room temperature cures or faster elevated temperature cures.
- Good abrasion resistance, tough, high strength coatings, liners and adhesive/sealants.
- High bond strength to a wide variety substrates.
- Low thermal expansion coefficient.
Information provided by MasterBond® |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |