MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silres® MSE 100 Methylsilicate
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® MSE 100 is the methyl ester of a mixture of different oligomeric methylsilicates. It is a methoxyfunctional methyl polysiloxane.

Properties: SILRES® MSE 100 is recommended as an ambient temperature moisture-curing binder for heat resistant paints. In combination with suitable catalysts and temperature stable pigments and fillers, SILRES® MSE 100 is the optimum binder for ambient curing, heat resistant paints. The curing rate depends on the catalyst used and on the relative humidity. After paint application and paint drying, coatings based on SILRES® MSE 100 can withstand temperatures of up to 650°C (1200°F) without loosing adhesion.

Special features:

  • low viscous liquid, solvent free silicone binder (solvent content < 2%)
  • very high inorganic content (corresponds to 68 - 72% SiO2)
  • curable at ambient temperature within less than 15min
  • almost no smoke generation upon initial stoving
  • limited compatibility (preferably used as a sole binder)
Application: SILRES® MSE 100 is the binder of choice for all heat resistant coatings between 200°C (400°F) and 650°C (1200°F) which have to cure at ambient temperature prior to heat exposure. In many applications the major target of the coating is to provide corrosion resistance to the steel or aluminum substrate. Corrosion resistance can be further improved if a zinc-rich ethylsilicate is used as a primer (thereby lowering maximum operation temperature to around 420°C). Maximum heat resistance depends on the paint formulation, especially on the pigments used. A maximum temperature up to 650°C (1200°F) is observed for silver-coloured aluminum pigments and about 500°C (930°F) for black pigments. Others colors are possible as well.
  • automotive, motor-bike and aircraft parts (e. g. exhaust systems, mufflers, engine parts)
  • industrial coatings (Chimneys, furnaces, gas boilers, heat exchangers, light bulbs)
  • household & appliances (ovens (inserts), stoves, barbecues)

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
Kinematic Viscosity 20 - 35 cSt20 - 35 cStDIN 51562
 
Thermal PropertiesMetricEnglishComments
Flash Point 69.0 °C156 °FISO 3679
Ignition Temperature 220 °C428 °F
 
Descriptive Properties
Appearanceclear low-viscous liquid
Colorcolorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poco Graphite PYROGRAPH Ion Implant Grade Graphite
Hybrid Plastics POSS® MA0704 MethacrylCyclohexyl-POSS®
Hybrid Plastics POSS® MA0702 MethacrylIsobutyl-POSS®
Hybrid Plastics MS0825 Nanoreinforced® POSS® Polypropylene
Hybrid Plastics MS0825 Nanoreinforced® POSS® Polyamide 6

PWACK9581 / 205110

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.