MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Westlake Epolene® C-13P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Epolene C-13P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and to provide lubricity in rubber compounding. Coatings produced with Epolene C-13P exhibit high gloss, low moisture vapor transmission rates, grease resistance, and good heat seal ability.
    Key Attributes:
  • Enhances paraffin wax coating properties like gloss, grease resistance, and MVTR
  • Excellent thermal stability
  • Low color
  • Medium molecular weight
  • Useful in color concentrates
    Application/Uses:
  • Automotive refinish
  • Building and Construction
  • Hot Melt Adhesives
  • Inks
  • Packaging
  • Solvent borne Adhesives
  • Wax Modification

    Information provided by Westlake Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 - 0.920 g/cc
Brookfield Viscosity 190 cP
@Load 2.16 kg,
Temperature 190 °C
Molecular Weight 76000 g/mol
Melt Flow 160 - 240 g/10 min72-412
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 343 °CASTM E136
Ring & Ball Softening Point 110 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0542-130
 
Descriptive Properties
Penetration Hardness3 dmmASTM D5, Needle under 100-g load for 5s @ 25 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 1
Silicon Nitride
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
AISI 1005 Steel
Westlake Epolene® C-13 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer

PWESF8902 / 133447

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.