Grade MC223 is a medium weave cotton phenolic composite. Typical applications include pintle and stave-type bearings for rudder shafts in the marine industry. This material is known industry wide as “Marine Micarta.” This product is also suitable for heavy equipment applications that require finer machining profiles than those provided by bearing-grade laminates.Information provided by Norplex-Micarta |
Cotton, Phenolic, Micarta, Marine Micarta, Bearings |