ATI Allegheny Ludlum AM 350™ High Strength Specialty Steel Alloy, UNS S35000
Categories:
Metal
;
Ferrous Metal
;
Stainless Steel
;
T 300 Series Stainless Steel
Material Notes:
Property data below is typical of annealed samples. Available in sheet and strip only. For use in valves, aircraft tubing, bellows, mounts, brackets, and ducts.
Information provided by Allegheny Ludlum
Key Words:
ASTM A-693; ASME SA-693; AMS 5548
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
7.81
g/cc
0.282
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell B
100
100
Tensile Strength, Ultimate
1175
MPa
170400
psi
Tensile Strength, Yield
485
MPa
@Strain 0.2 %
70300
psi
@Strain 0.2 %
Elongation at Break
30 %
30 %
Component Elements Properties
Metric
English
Comments
Chromium, Cr
16.5 %
16.5 %
Iron, Fe
76 %
76 %
as balance
Manganese, Mn
0.80 %
0.80 %
Molybdenum, Mo
2.75 %
2.75 %
Nickel, Ni
4.3 %
4.3 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
AM-350 Stainless Steel Plate, Sheet, Strip, Condition H850, UNS S35000
Universal Wire Works AM350 (AMS 5774) Filler Metal
AM-350 Stainless Steel, Annealed Plate, Sheet, Strip, UNS S35000
AISI M1015 Merchant Quality Carbon Steel, Composition Spec
AISI 4626 Steel
NL350 / 17886
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.