MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chase Electronic Coatings HumiSeal® UV92 UV Curable masking Material
Categories: Polymer; Thermoset

Material Notes: HumiSeal® UV92 is a soft, one part, UV curable masking material. HumiSeal® UV92 applies easily because of its shearing thinning viscosity profile and is 100% cured by exposure to UV to provide a temporary barrier to prevent ingress of coatings into keep out areas. HumiSeal® UV92 has excellent solvent resistance that provides selective release from conformal coating. HumiSeal® UV92 will survive intermittent exposure to temperatures up to 150°C. HumiSeal® UV92 is REACH and RoHS compliant and available in bulk and syringes. Applies easily by syringes, dispensing machines. Keeps contact points and connections free of coating. Will not tarnish gold, tin, copper, phosphor bronze and Sn/Pb solder. Easily removed by peeling - leaves no residue to interfere with subsequent operations.

Recommended cure: UV-LED at 365 nm. "H" type microwave (minimum power of 200nW/cm2): UV-LED at 365 nm. "H" type microwave (minimum power of 200nW/cm2)

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
Elongation at Break >= 200 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
Glass Transition Temp, Tg -50.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 8.00 - 28.0 °C
DOM
 
Descriptive Properties
AppearanceThixotropic paste
Colormilky white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHAS957 / 239818

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.