MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sipol Technipol® 9 Thermoplastic Linear Polyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Description: Technipol® 9 is a thermoplastic linear polyester based on polybutylene terephthalate. Technipol® 9 has been specifically developed, with its unique rheological behavior and chemical compatibility with PET, to fulfill the demanding needs of masterbatch carriers. Technipol® 9 is characterized by excellent mechanical and electrical properties, good chemical resistance and good dimensional stability. Technipol® 9 comes in a natural color, fully in compliance with American FDA and European EU 10/2011 Food Contact Regulations.

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D 792
Melt Flow 38 g/10 min
@Load 2.16 kg,
Temperature 250 °C
38 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D 1238
Storage Temperature 5.00 - 10.0 °C41.0 - 50.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FASTM D 3418
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPOL036 / 297161

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.