MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® F-562 Phenolic Prepreg, C2 Carbonized Rayon Reinforced
Categories: Polymer; Thermoset; Phenolic

Material Notes: Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environments.

Key Features and Benefits:

  • Provides a combination of high-strength and ablative properties for demanding applications
  • Low thermal expansion
  • Good Tack and Drape properties
  • Highly toughened resin system for improved impact resistance

Applications/Qualifications:

  • Rocket Nozzles
  • Combustion Chambers
  • Heat Shields
  • Exhaust Gas Management

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 2.0 - 4.0 %
@Temperature 135 °C
8 min
Thickness 15.0 milnominal, cured, per ply
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 7800 psi
@Temperature 23.9 °C
±45° Direction, Dry; ASTM D638
 38000 psi
@Temperature 23.9 °C
0° Direction, Dry; ASTM D638
Elongation at Yield 7.2 %
@Temperature 23.9 °C
Tensile; Dry; ASTM D638
Tensile Modulus 400 ksi
@Temperature 23.9 °C
±45° Direction, Dry; ASTM D638
 1800 ksi
@Temperature 23.9 °C
0° Direction, Dry; ASTM D638
Flexural Strength 30.0 ksi
@Temperature 23.9 °C
Dry; ASTM D790
Flexural Modulus 1600 ksi
@Temperature 23.9 °C
Dry; ASTM D790
Compressive Strength 19.0 ksi
@Temperature 23.9 °C
Dry; ASTM D695
Compressive Modulus 1800 ksi
@Temperature 23.9 °C
Dry; ASTM D695
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 4.44 °C
 
Descriptive Properties
Resin Flow (%)1-7260°F, 150psi
Resin Solids Content (%)30-36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade
Covestro Baytec® ENC-55P Polyurethane
Mitsubishi Rayon Acrypet® IR H70 Impact Modified PMMA
Overview of materials for Cellulose Acetate Butyrate, Molded
Overview of materials for Phenolic, Novolac, Cellulose Filled

PPARK062 / 89334

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.