MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Super ATF Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Super ATF is a high-quality transmission fluid recommended for use in all domestic and import vehicles no longer under warranty where the OEM previously specified a GM DEXRON®-III H or Ford MERCON® fluid. Super ATF is formulated to provide the proper frictional characteristics for smooth, quiet shifting in electronically controlled automatic transmissions. It has excellent oxidation resistance for long fluid life, excellent low-temperature properties for easy shifting in cold weather, protects against wear and helps minimize the formation of sludge and varnish.

Applications:

  • GM and Ford automatic transmissions in 2005 and earlier model-year vehicles that are no longer under warranty, where the OEM previously specified DEXRON® -III H, DEXRON®-II, DEXRON® or MERCON® ATF
  • Import vehicles where DEXRON®-III H (obsolete) or an earlier-generation DEXRON® fluid (obsolete) is specified
  • Allison heavy-duty off-highway automatic transmissions that require a C-4 quality fluid
  • Hydraulic systems on industrial and mobile equipment operating over a wide temperature range
Features/Benefits:
  • Proper frictional properties for smooth shifting and excellent anti-shudder performance
  • Excellent thermal stability and oxidation resistance for long fluid life
  • Excellent low-temperature properties
  • Protects against wear
  • Minimizes sludge and varnish deposits
  • Protects against rust and corrosion
  • Good seal compatibility
  • Suitable for both automotive and industrial applications

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.861 g/cc0.861 g/cc
Density 0.859 g/cc0.0310 lb/in³
Brookfield Viscosity 14000 cP
@Temperature -40.0 °C
14000 cP
@Temperature -40.0 °F
Viscosity Measurement 188188Index
Kinematic Viscosity at 40°C (104°F) 32.1 cSt32.1 cSt
Kinematic Viscosity at 100°C (212°F) 7.0 cSt7.0 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -40.0 °C<= -40.0 °F
Flash Point 212 °C414 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn <= 0.0030 %<= 0.0030 %
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5024 / 198277

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.