System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Durethan® B 30 S FN30 000000 Nylon 6 (PA6), Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Unreinforced
Material Notes:
PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistance
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.14
g/cc
0.0412
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
2.8 %
2.8 %
50% RH; ISO 62
Water Absorption at Saturation
8.9 %
8.9 %
ISO 62
Linear Mold Shrinkage, Flow
0.0090
cm/cm
0.0090
in/in
60x60x2; 260 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0090
cm/cm
0.0090
in/in
60x60x2; 260 °C / MT 80°C; 600 bar; ISO 294-4
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
150
MPa
21800
psi
ISO 2093-1
Tensile Strength at Break
80.0
MPa
11600
psi
5 mm/min; ISO 527-1,-2
Tensile Strength, Yield
80.0
MPa
11600
psi
50 mm/min; ISO 527-1,-2
Elongation at Break
10 %
10 %
50 mm/min, Nominal; ISO 527-1,-2
14 %
14 %
5 mm/min; ISO 527-1,-2
Elongation at Yield
3.5 %
3.5 %
50 mm/min; ISO 527-1,-2
Tensile Modulus
3.70
GPa
537
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
120
MPa
17400
psi
2 mm/min; ISO 178-A
Flexural Yield Strength
110
MPa
@Strain 3.5 %
16000
psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
3.60
GPa
522
ksi
2 mm/min; ISO 178-A
Flexural Strain at Break
2.5 %
2.5 %
2 mm/min; ISO 178-A
Izod Impact, Unnotched (ISO)
65.0
kJ/m²
@Temperature -30.0 °C
30.9
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
90.0
kJ/m²
@Temperature 23.0 °C
42.8
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched
7.50
J/cm²
@Temperature -30.0 °C
35.7
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
9.00
J/cm²
@Temperature 23.0 °C
42.8
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched
<=
1.00
J/cm²
@Temperature 23.0 °C
<=
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+13
ohm-cm
1.00e+13
ohm-cm
IEC 60093
Surface Resistance
1.00e+16
ohm
1.00e+16
ohm
IEC 60093
Comparative Tracking Index
0.00
V
0.00
V
Solution A; UL 746A
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
70.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow
80.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point
222
°C
432
°F
10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air
207
°C
405
°F
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
185
°C
365
°F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
65.0
°C
149
°F
ISO 75-1,-2
Flammability, UL94
V-0
@Thickness 0.380 mm
V-0
@Thickness 0.0150 in
V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index
40 %
40 %
Method A; ISO 4589-2
Glow Wire Ignition Temperature
775
°C
@Thickness 1.50 mm
1430
°F
@Thickness 0.0591 in
IEC 60695-2-13
775
°C
@Thickness 3.00 mm
1430
°F
@Thickness 0.118 in
IEC 60695-2-13
960
°C
@Thickness 0.400 mm
1760
°F
@Thickness 0.0157 in
IEC 60695-2-13
960
°C
@Thickness 0.750 mm
1760
°F
@Thickness 0.0295 in
IEC 60695-2-13
Glow Wire Flammability Index
960
°C
@Thickness 0.400 mm
1760
°F
@Thickness 0.0157 in
IEC 60695-2-12
960
°C
@Thickness 0.750 mm
1760
°F
@Thickness 0.0295 in
IEC 60695-2-12
960
°C
@Thickness 1.50 mm
1760
°F
@Thickness 0.0591 in
IEC 60695-2-12
960
°C
@Thickness 3.00 mm
1760
°F
@Thickness 0.118 in
IEC 60695-2-12
Shrinkage, MD
0.30 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.30 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Flow Direction Post-Molding, 60x60x2; ISO 294-4
Shrinkage, TD
0.30 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.30 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Molding, 60x60x2; ISO 294-4
Processing Properties
Metric
English
Comments
Melt Temperature
260
°C
500
°F
injection molding; ISO 294
250
-
270
°C
482
-
518
°F
Mold Temperature
80.0
°C
176
°F
injection molding; ISO 294
80.0
-
100
°C
176
-
212
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
-
6.00
hour
2.00
-
6.00
hour
Moisture Content
0.030 - 0.070 %
0.030 - 0.070 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Envalior Durethan® B 30 S F30 000000 Nylon 6 (PA6), Dry
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural
Domo TECHNYL® PSB 286 PA6, DRY
Envalior Durethan® B 30 S 000000 Nylon 6 (PA6), Dry
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
PLANW9260 / 208061
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.