MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® A3 GF 30 4 L black (4678) PA 6 Dry, 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: AKROMID® Lite and AKROMID® XtraLite bridge the gap between polypropylene and polyamide. In comparison to polypropylene, AKROMID ® Lite and AKROMID® XtraLite display a superior surface quality, enhanced mechanical properties and higher heat resistance. In comparison to PA6 compounds, AKROMID ® Lite and AKROMID® XtraLite score higher in terms of lower density, lower volume price, superior flowability, reduced moisture absorption and enhanced notched impact strength. The objective of the AKROPLASTIC developers was to create a technical polyamide compound with a lower density while maintaining the typical properties of polyamide.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Filler Content 30 %30 %ISO 1172
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 150 MPa21800 psi5 [mm/min]; ISO 527-2
Elongation at Break 2.8 %2.8 %5 [mm/min]; ISO 527-2
Tensile Modulus 8.60 GPa1250 ksi1 [mm/min]; ISO 527-2
Flexural Strength 220 MPa31900 psi2 [mm/min]; ISO 178
Flexural Modulus 8.60 GPa1250 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FDIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 246 °C475 °FHDT/A; ISO 75
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Nozzle Temperature 270 - 290 °C518 - 554 °F
Zone 1 230 - 295 °C446 - 563 °F
Zone 2 230 - 295 °C446 - 563 °F
Zone 3 230 - 295 °C446 - 563 °F
Zone 4 230 - 295 °C446 - 563 °F
Melt Temperature 270 - 295 °C518 - 563 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time <= 2.00 hour<= 2.00 hour
Hold Pressure 30.0 - 80.0 MPa4350 - 11600 psi
Back Pressure 50.0 MPa7250 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 GF 30 4 L black (4678) PA 6 Conditioned, 30% Glass Filled
Akro-Plastic Akromid® B3 GF 30 S1 BLACK (1281) PA, Cold-Impact Resistant, 30% Glass Filled, Black
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Conditioned, 30% Glass Filled
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled

PAKRO163 / 182750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.