Bada BADAMID® PA610 GF/CF20 TM-Z1 black PA610, 20% Glass/Carbon Reinforced, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 610 (PA610)
;
Nylon 610, Carbon Fiber Filled
;
Nylon 610, Glass Reinforced
Material Notes:
30% glass fiber and carbon fiber reinforced PA610 compound for injection molding, impact resistant modified with excellent mechanical characteristics
Information provided by Bada
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.20
g/cc
0.0434
lb/in³
ISO 1183
Moisture Absorption
0.600 %
0.600 %
50% r.h.; ISO 62
Water Absorption at Saturation
1.4 %
1.4 %
ISO 62
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
130
MPa
18900
psi
5 mm/min; ISO 527-1/2
Elongation at Break
4.0 %
4.0 %
5 mm/min; ISO 527-1/2
Tensile Modulus
8.50
GPa
1230
ksi
1 mm/min; ISO 527-1/2
Charpy Impact Unnotched
8.50
J/cm²
@Temperature 23.0 °C
40.4
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.700
J/cm²
@Temperature -30.0 °C
3.33
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
1.00
J/cm²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1000
ohm-cm
1000
ohm-cm
IEC-62631-3-1
Surface Resistance
1000
ohm
1000
ohm
IEC-62631-3-2
Comparative Tracking Index
550
V
550
V
IEC-60112
Thermal Properties
Metric
English
Comments
Melting Point
220
°C
428
°F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi)
210
°C
410
°F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi)
200
°C
392
°F
ISO 75-1/2
Flammability, UL94
HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Processing Properties
Metric
English
Comments
Melt Temperature
270
-
290
°C
518
-
554
°F
Mold Temperature
80.0
-
90.0
°C
176
-
194
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Moisture Content
<= 0.15 %
<= 0.15 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PBADA270 / 287103
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.