  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials Vespel® SMP-40025 DF Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: Parts from graphite filled PI (polyimide) for high thermal and oxidative stability with high modulus and dimensional stability at high temperatures and loads.

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D 792
Water Absorption 0.18 %0.18 %Immersion 24h; ASTM D 570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  52.0 MPa
@Temperature 260 °C
7540 psi
@Temperature 500 °F
ASTM D 638
 102 MPa
@Temperature 23.0 °C
14800 psi
@Temperature 73.4 °F
ASTM D 638
Elongation at Break  1.8 %
@Temperature 23.0 °C
1.8 %
@Temperature 73.4 °F
ASTM D 638
 7.9 %
@Temperature 260 °C
7.9 %
@Temperature 500 °F
ASTM D 638
Tensile Modulus 5.994 GPa
@Temperature 23.0 °C
869.4 ksi
@Temperature 73.4 °F
ASTM D 638
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 417 °C783 °FASTM D 648
 
Descriptive Properties
FillerGraphite Powder
Heat StabilizedYes
Polymer FamilyPolyimide
Polymer TypePI
Region AvailableAmericas
 Asia/Pacific
 Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
DuPont Mobility and Materials Vespel® SCP-50094 Polyimide
CRG Industries Essemplex AF34 Thermoplastic Shape Memory Polymer Resin
CRG Industries Essemplex AB43 Thermoplastic Shape Memory Polymer Resin

PDTA7750 / 89861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.