MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Lupox® LW-5402 Low Warpage PBT, 40% Glass Filled, High Impact  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled

Material Notes: LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. LUPOX resins show minimal moisture absorption, excellent electrical properties, plus good chemical resistance against water, weak acid and many solvents.

Applications:

    Automotive: Back beam, door frame garnish, distributor cap, rotor arm, head lamp actuator, bezel, door handle, ignition components, connectors, speed control device, window drive system

    Electrical and Electronic: Relay, lamp socket, solenoid and transformer bobbin, timer case, focus pack, refrigerator muffler, key top, condenser, switch, connector, electronic range door latch, zircon frame and blade, PC inlet socket

    Industrial Parts and Household Appliances: Pump case, oven handle, toaster and cooker housing, gear, insulator support and bracket, telecommunications cable splice closure, water meter housing, loose tube

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D792
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 95.0 MPa13800 psiASTM D638
Elongation at Break 7.0 %7.0 %ASTM D638
Flexural Strength 150 MPa21800 psiASTM D790
Flexural Modulus 7.80 GPa1130 ksiASTM D790
Izod Impact, Notched 0.750 J/cm
@Temperature 23.0 °C
1.41 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 245 °C446 - 473 °F
Middle Barrel Temperature 235 - 250 °C455 - 482 °F
Front Barrel Temperature 240 - 260 °C464 - 500 °F
Nozzle Temperature 240 - 260 °C464 - 500 °F
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 50.0 - 100 °C122 - 212 °F
Drying Temperature  120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
dehumidifying dryer
 140 °C
@Time 7200 sec
284 °F
@Time 2.00 hour
dehumidifying dryer
Injection Pressure 39.23 - 83.36 MPa5690 - 12090 psiSecond
 68.7 - 118 MPa9960 - 17100 psiFirst
Back Pressure 0.000 - 3.92 MPa0.000 - 569 psi
Screw Speed 40 - 75 rpm40 - 75 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity
Avient Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT)
Overview of materials for AISI 4000 Series Steel
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release

PLGCHEM022 / 50843

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.