MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 10% Glass Fiber Reinforced

Material Notes: Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibility with SMT processes, and low moisture absorption. - White: A-1133 NL WH 886

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0582 lb/in³ISO 1183/A
Water Absorption 0.12 %
@Time 86400 sec
0.12 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 125125R-Scale; ASTM D785
Tensile Strength 120 MPa17400 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Tensile Modulus 9.17 GPa1330 ksiASTM D638
Flexural Strength 175 MPa25400 psiASTM D790
Flexural Modulus 7.52 GPa1090 ksiASTM D790
Poissons Ratio 0.410.41ASTM E132
Shear Modulus 3.25 GPa471 ksiCalculated
Izod Impact, Notched 0.270 J/cm0.506 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  20.0 µm/m-°C
@Temperature 160 - 249 °C
11.1 µin/in-°F
@Temperature 320 - 480 °F
TMA; ASTM E831
 25.0 µm/m-°C
@Temperature 0.000 - 100 °C
13.9 µin/in-°F
@Temperature 32.0 - 212 °F
TMA; ASTM E831
CTE, linear, Transverse to Flow  41.0 µm/m-°C
@Temperature 0.000 - 100 °C
22.8 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E228
 65.0 µm/m-°C
@Temperature 160 - 249 °C
36.1 µin/in-°F
@Temperature 320 - 480 °F
ASTM E228
Melting Point 325 °C617 °FASTM D570
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 304 - 318 °C579 - 604 °F
Front Barrel Temperature 316 - 329 °C601 - 624 °F
Melt Temperature 321 - 343 °C610 - 649 °F
Mold Temperature 135 °C275 °F
Drying Temperature 120 °C248 °F
Dry Time 4.00 hour4.00 hour
Moisture Content 0.060 %0.060 %
 
Descriptive Properties
AppearanceWhite
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
FeaturesGood Chemical Resistance
 Good Color Stability
 High Reflectivity
 Low Moisture Absorption
FillerGlass Fiber Reinforcement
FormsPellets
GenericPPA
Processing MethodInjection Molding
UsesAutomotive Electronics
 LEDs

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Carbon Steel

PSOL8Y7511 / 135591

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.