MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

REXtac Rextac® RT 2115 Amorphous Polyalphaolefin (APAO)
Categories: Polymer; Thermoplastic; Polyalphaolefin; Polyolefin

Material Notes:
Adhesive and Sealant Grade.

Description: Propylene homopolymer and FDA compliant

Features: High softening point and short open time

Applications: Component of hot melt adhesives, sealants and specialty products

Other Properties:
Ring and Ball Softening Point (ASTM E 28): 152°C.
Needle Penetration (ASTM D 1321): 15 mm.
Shear Adhesion Failure Temperature (SAFT), Kraft/Kraft (Huntsman Method): 132°C.
Open Time, Kraft/Kraft (Huntsman Method): 0 sec.
Melt Density (190°C; Huntsman Method): 0.74 g/cc.
Flashpoint, COC (ASTM D 93): >235°C.

Information provided by Huntsman Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 g/cc0.0311 lb/in³ASTM D 792
Melt Density  0.740 g/cc
@Temperature 190 °C
0.0267 lb/in³
@Temperature 374 °F
 0.740 g/cc
@Temperature 190 °C
0.0267 lb/in³
@Temperature 374 °F
Viscosity  1500 cP
@Temperature 190 °C
1500 cP
@Temperature 374 °F
Melt; ASTM D-3236
 1500 cP
@Temperature 190 °C
1500 cP
@Temperature 374 °F
Melt
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2.30 MPa334 psiASTM D-638, D-412
 2.30 MPa334 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 132 °C270 °FShear Adhesion Failure Temperature (SAFT), Kraft/Kraft; Huntsman Method
 132 °C270 °FShear Adhesion Failure Temperature (SAFT), Kraft/Kraft; Huntsman Method
Glass Transition Temp, Tg -20.0 °C-4.00 °FASTM D-3418
 -20.0 °C-4.00 °F
Flash Point >= 235 °C>= 455 °FCOC; ASTM D 93
 >= 235 °C>= 455 °FCOC; ASTM D 93
Ring & Ball Softening Point 152 °C306 °FASTM E 28
 152 °C306 °FASTM E 28
 
Processing PropertiesMetricEnglishComments
Pot Life <= 0.0833 min<= 0.0833 minOpen Time; ASTM D-4497
 <= 0.0833 min<= 0.0833 minOpen Time, Kraft/Kraft; Huntsman Method
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 YesYes
 
Descriptive Properties
Needle Penetration (mm)15ASTM D 1321

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 3640 EPDM Hydrocarbon Rubber
Lanxess Keltan® 2450 Ethylene-Propylene Rubber
Versalis Dutral® CO 054 Ethylene - Propylene
Eastman 1810A Polyethylene
ICO Polymers ICORENE™ 155-1326 LMDPE Rotational Molding Resin

PHUN00 / 47620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.