MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formulated long term UV stability package in pellet form.

Applications: Large agricultural tanks; Industrial products.

Key Words: Linear High Density Polyethylene; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³Exxon Method
Environmental Stress Crack Resistance 200 hour200 hourF50, Condition B; ASTM D-1693
Melt Flow 2.0 g/10 min2.0 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.6 MPa2700 psiASTM D638
Elongation at Break 350 %350 %ASTM D638
Flexural Modulus 0.710 GPa103 ksiASTM D790
Impact Test 237 J
@Thickness 6.35 mm,
Temperature -40.0 °C
175 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °FExxon Method
Deflection Temperature at 0.46 MPa (66 psi) 54.5 °C130 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C108 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 8760.29 Rotational Molding Resin
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
NOVA Chemicals SURPASS® RMs245-U sHDPE Rotational Molding Resin
ExxonMobil HD 8660.29 Rotational Molding Resin

PEXCFW / 37944

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.