MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® 2 Adhesive Accelerator
Categories: Fluid; Other Engineering Material; Catalyst/Initiator

Material Notes: Quick Tac Accelerators have been developed as a treating agent for use with the ADVANCED PERFORMANCE family of instant adhesive products. If faster setting speeds are desired, QUICK TAC will aid the curing process and give exceptionally faster set times. When curing beads or in applications where the adhesive is not between two parts, it will allow for faster uniform curing. QUICK TAC will aid the bonding of porous materials such as fabrics or woods. It is useful when bonding acidic surfaces or in low humidity conditions promoting consistent curing times. Used for wire tacking , silk screening , or in loudspeaker assembly. Using QUICK TAC will enable the adhesive to fill gaps up to 0.20". QUICK TAC can be applied by brushing or spraying.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.790 g/cc0.790 g/cc
Viscosity 3.0 cP3.0 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point 56.1 °C133 °F
Flash Point <= -17.8 °C<= 0.000 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthIn original sealed container when properly stored.
 
Descriptive Properties
Baseacetone
Color / appearanceclear/amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Addocat® DB PU Catalyst/Activator
Lanxess Addocat® 201 PU Catalyst/Activator

PASINC9074 / 233441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.