MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials Duratron™ DU7000 PI Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: This robust, compression molded PI offers outstanding electrical, thermal, and mechanical properties in high temperature applications, helping to extend service life and increase uptime.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Water Absorption at Saturation 1.50 %1.50 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 120120ASTM D785
Tensile Strength 140 MPa20300 psiISO 527-1/-2 (7)
Flexural Strength 190 MPa27600 psiISO 178 (12)
Compressive Yield Strength  45.0 MPa
@Strain 1.00 %
6530 psi
@Strain 1.00 %
ISO 604 (10)
 90.0 MPa
@Strain 2.00 %
13100 psi
@Strain 2.00 %
ISO 604 (10)
 170 MPa
@Strain 5.00 %
24700 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C40.0 µin/in-°FASTM E-831 (TMA)
 40.0 µm/m-°C
@Temperature 23.0 - 150 °C
22.2 µin/in-°F
@Temperature 73.4 - 302 °F
 52.0 µm/m-°C
@Temperature >=150 °C
28.9 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.360 W/m-K2.50 BTU-in/hr-ft²-°F
 0.360 W/m-K2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °FContinuous Use Temperature in Air after 20000 hr
Minimum Service Temperature, Air -196 °C-321 °F
 -196 °C-321 °F
Glass Transition Temp, Tg 291 °C555 °FDMA- Tan d
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak AcceptableAcceptable
Alcohols UnacceptableUnacceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak UnacceptableUnacceptable
Chlorinated Solvents UnacceptableUnacceptable
Continuous Sunlight UnacceptableUnacceptable
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic UnacceptableUnacceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SMU765 / 323880

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.