MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Akulon® XP32-E1 PA6
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: Film Extrusion, Medium Viscosity, Lubricated, Nucleated

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Vapor Transmission 35.0 g/m²/day
@Temperature 23.0 °C
2.25 g/100 in²/day
@Temperature 73.4 °F
at 85% r.h., Film; DIS 15106-1/-3
Oxygen Transmission  1.05 cc-mm/m²-24hr-atm
@Temperature 23.0 °C
2.67 cc-mil/100 in²-24hr-atm
@Temperature 73.4 °F
at 0% r.h., Film; DIS 15105-1/-2
 1.55 cc-mm/m²-24hr-atm
@Temperature 23.0 °C
3.94 cc-mil/100 in²-24hr-atm
@Temperature 73.4 °F
at 85% r.h., Film; DIS 15105-1/-2
Viscosity 1.45e+6 cP
@Temperature 260 °C
1.45e+6 cP
@Temperature 500 °F
Melt Viscosity; DSM Method
 200000 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
200000 cP
@Shear Rate 1000 1/s,
Temperature 536 °F
 250000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
250000 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
 300000 cP
@Shear Rate 1000 1/s,
Temperature 240 °C
300000 cP
@Shear Rate 1000 1/s,
Temperature 464 °F
 1.00e+6 cP
@Shear Rate 0.1 1/s,
Temperature 280 °C
1.00e+6 cP
@Shear Rate 0.1 1/s,
Temperature 536 °F
 2.00e+6 cP
@Shear Rate 0.1 1/s,
Temperature 260 °C
2.00e+6 cP
@Shear Rate 0.1 1/s,
Temperature 500 °F
 3.00e+6 cP
@Shear Rate 0.1 1/s,
Temperature 240 °C
3.00e+6 cP
@Shear Rate 0.1 1/s,
Temperature 464 °F
Viscosity Measurement 2.82.8RSV formic acid, 1g/100ml; DSM Method
Viscosity Number 177 cm³/g1.77 dl/gISO 307, 1157, 1628
Thickness 50.0 microns1.97 milFilm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 36.0 MPa5220 psiparallel; ISO 527-3
Film Elongation at Break, MD 340 %340 %parallel; ISO 527-3
Modulus of Elasticity 0.490 GPa71.1 ksiFilm; DSM-Method, 50mm/min
Coefficient of Friction, Dynamic 0.800.80Film; ISO 8295
Coefficient of Friction, Static 1.41.4Film; ISO 8295
Tear Strength Test 2323Trouser Tear Resistance, parallel, Film; ISO 6383-1
Film Tensile Strength at Break, MD 96.0 MPa13900 psiparallel; ISO 527-3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
Specific Heat Capacity  1.55 J/g-°C
@Temperature 23.0 °C
0.370 BTU/lb-°F
@Temperature 73.4 °F
 2.55 J/g-°C
@Temperature 20.0 - 150 °C
0.609 BTU/lb-°F
@Temperature 68.0 - 302 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 85 %85 %Film; DSM Method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 °C518 °FExtruder Temperature, Film
Die Temperature 270 °C518 °F
Roll Temperature 110 °C230 °F
 
Descriptive Properties
Extrusion TypeCast Film
Puncture Resistance1200 J/mFilm (DSM Method)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell RZ-18 Copolymer Polypropylene, 40% Calcium Carbonate Filled
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced
Adell RQ-18 Copolymer Polypropylene, 40% Mica Reinforced
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled
Afton Plastics 350 PFA Welding Rod

PDSM9703 / 161324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.