MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Angst+Pfister APSOplast® PE-UHMW Regenerat Ultra-high molecular hard PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: PE-UHMW, often also called PE-1000, has very good sliding and wear properties. The molecular mass (weight) ranges from around 4.5 to 9.0 · 106 g/mol. This material combines excellent wear resistance with exceptional impact resistance, even at temperatures below –200°C. Due to its really low moisture absorption, PE-UHMW is particularly dimensionally stable.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 0.940 g/cc>= 0.0340 lb/in³DIN EN ISO 1183-1
Moisture Absorption <= 0.0100 %<= 0.0100 %50 % r.h.; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62 - 6762 - 67DIN EN ISO 868
Ball Indentation Hardness 36.0 MPa5220 psiDIN EN ISO 2039-1
Tensile Strength >= 20.0 MPa>= 2900 psi50 mm/min; DIN EN ISO 527
Tensile Strength, Yield >= 20.0 MPa>= 2900 psi50 mm/min; DIN EN ISO 527
Elongation at Break >= 50 %>= 50 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity >= 0.700 GPa>= 102 ksi1 mm/min; DIN EN ISO 527
Charpy Impact, Notched 10.0 J/cm²47.6 ft-lb/in²ISO 11542-2
Coefficient of Friction 0.10 - 0.160.10 - 0.16against hardened and polished steel; ASTM D 1894
Abrasion 120 - 140120 - 140PE-UHMW, natural = 100%, (Sand-Slurry-Test); ISO 15527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+14 ohm-cm<= 1.00e+14 ohm-cmIEC 60093
Surface Resistance <= 1.00e+13 ohm<= 1.00e+13 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C111 µin/in-°FDIN 53752
Thermal Conductivity 0.410 W/m-K2.85 BTU-in/hr-ft²-°F
Melting Point 133 - 137 °C271 - 279 °FISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C176 °Flong term
Flammability, UL94 HBHB
 
Descriptive Properties
Colorcolored

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP007 / 250505

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.