MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Arkema Pebax® MV 1074 SA 01 TPA
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyether Block Amide (PEBA)

Material Notes:

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Moisture Absorption 1.40 %1.40 %Dry; Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 40
@Time 15.0 sec
40
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength at Break 30.0 MPa4350 psiDry; ISO 527-1/-2
Film Elongation at Break, MD 500 %500 %Dry; ISO 527-3
Film Elongation at Break, TD 700 %700 %Dry; ISO 527-3
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Cond.; ISO 527-1/-2
 >= 300 %>= 300 %Dry; ISO 527-1/-2
Tensile Modulus 0.0800 GPa11.6 ksiCond.; ISO 527-1/-2
 0.0970 GPa14.1 ksiDry; ISO 527-1/-2
50% Modulus  10.0 MPa
@Strain 50 %
10.0 MPa
@Strain 50 %
Dry; ISO 527-1/-2
 10.0 MPa
@Strain 50 %
10.0 MPa
@Strain 50 %
Cond.; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eA
Film Tensile Strength at Break, MD 32.0 MPa4640 psiDry; ISO 527-3
Film Tensile Strength at Break, TD 34.0 MPa4930 psiDry; ISO 527-3
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.50e+9 ohm-cm2.50e+9 ohm-cmCond.; IEC 60093
 1.50e+11 ohm-cm1.50e+11 ohm-cmDry; IEC 60093
Surface Resistance 3.00e+9 ohm3.00e+9 ohmCond.; IEC 60093
Dielectric Strength 5.00 kV/mm127 kV/inDry; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 158 °C316 °F10°C/min; Dry; ISO 11357-1/-3
Glass Transition Temp, Tg -40.0 °C-40.0 °F10°C/min; Dry; ISO 11357-1/-2
Oxygen Index 19 %19 %Dry; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °FInjection Molding; ISO 294
Mold Temperature 30.0 °C86.0 °FInjection Molding; ISO 10724
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Hold Pressure 30.0 MPa4350 psiInjection Molding; ISO 294
 
Descriptive Properties
Anti-StaticYes
Form as DeliveredPellets
Heat StabilizedYes
Moisture SensitiveYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARKG726a / 291191

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.