MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Arlon R37806X030 Silicone Rubber/Fiberglass
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.80 g/cc2.80 g/ccsilicone property; Arlon SQA-TMS-024
Thickness 76.2 microns3.00 milside 1; Arlon SQA-TMS-003
 229 microns9.00 milside 2; Arlon SQA-TMS-003
 457 microns18.0 milsubstrate; Arlon SQA-TMS-003
 762 microns30.0 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7777silicone property; ASTM D2240
Tensile Strength, Ultimate 4.72 MPa685 psisilicone property; ASTM D412
Elongation at Break 125 %125 %silicone property; ASTM D412
Modulus of Elasticity 0.0245 GPa3.55 ksiArlon SQA-TMS-008
Poissons Ratio 0.500.50
Adhesive Bond Strength 0.0241 MPa3.50 psiArlon SQA-TMS-011
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 6.91
@Frequency 1e+6 Hz
6.91
@Frequency 1e+6 Hz
silicone property; IPC TM 650-2.5.5.3
Dielectric Strength 17.7 kV/mm450 kV/inASTM D149
Dissipation Factor 0.0044
@Frequency 1e+6 Hz
0.0044
@Frequency 1e+6 Hz
silicone property; IPC TM 650-2.5.5.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 111 µm/m-°C
@Temperature 20.0 °C
61.7 µin/in-°F
@Temperature 68.0 °F
silicone property; ASTM E 831
Specific Heat Capacity 0.820 J/g-°C
@Temperature 100 °C
0.196 BTU/lb-°F
@Temperature 212 °F
silicone property; Arlon SQA-TMS-052
Thermal Conductivity 1.40 W/m-K9.72 BTU-in/hr-ft²-°Fsilicone property; ASTM E1530
 1.54 W/m-K
@Temperature 100 °C
10.7 BTU-in/hr-ft²-°F
@Temperature 212 °F
overall; Arlon SQA-TMS-054
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -100 °C-148 °F
Glass Transition Temp, Tg -118 °C-180 °Fsilicone property; ASTM D3418
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 121 °C
0.250 hour
@Temperature 250 °F
 120 min
@Temperature 200 °C
2.00 hour
@Temperature 392 °F
Shelf Life 6.00 Month
@Temperature 7.22 °C
6.00 Month
@Temperature 45.0 °F
 
Descriptive Properties
ColorGray
Plasticity (mm) Arlon SQA-TMS-005silicone property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate
Rogers Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate
Rogers Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Epoxy Technology EPO-TEK® ED1021 Epoxy
Rogers Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

PARL064 / 79716

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.