MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Caplinq LINQTAPE™ PIT2SD 2 mil polyimide film with double-sided silicone adhesive and single release liner
Categories: Polymer; Adhesive; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: LINQTAPE™ PIT2SD-Series is a high performance, high-temperature resistant, pressure sensitive polyimide tape designed for both permanent and temporary bonding in many high temperature applications. These applications include but are not limited to semiconductor, smartcard, electronic, automotive and general manufacturing industries. LINQTAPE™ PIT2SD-Series provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 260°C(500°F). LINQTAPE™ PIT2SD-Series comes in 33meter (36yard) length rolls of varying widths. The base polyimide film (backing) thickness is 2mil (50.8±2µm) thick, has two silicone adhesive layers of 1.5mil (38.1µm) each and a single 3 mil (76.2µm) PET release liner on one side for a total thickness of approximately 8mil (203.2µm).

Applications:

  • High adhesion to wide range of substrates
  • Ideal for wafer dicing and die cutting
  • Temporary bonding of thermocouples for oven profiling
  • Bonding of devices prior to solder reflow
  • Splicing of Insulation layers
  • Masking in high temperature powder applications
  • Gold finger masking
  • Insulating circuit boards and coils
  • Wave solder masking tape
  • Insulation wrapping of coils, transformers and capacitors.

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 38.1 microns1.50 milAdhesive
 50.8 microns2.00 milFilm (Backing)
 76.2 microns3.00 milPET Release Liner
 203 microns8.00 milTotal
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 60 %>= 60 %
Tear Strength 8.90 kN/m50.8 plitensile, 1mil thick
Peel Strength 0.280 kN/m1.60 plito steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 217 kV/mm>= 5500 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 260 °C500 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
Adhesion TypeSilicone
ColorAmber
Insulation Class180 (H)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCAPL1006 / 256006

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.