MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Envalior ForTii® Eco E11 PPA-GF30 FR(40) PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® Eco E11 has an excellent balance in flow, toughness and stiffness with superior processing performance for injection molding. It has improved toughness and is suitable for SMT processes.

Features: Good or high flow, phosphorous free. 30% glass reinforced. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³Dry; ISO 1183
Moisture Absorption 1.40 %1.40 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0035 cm/cm0.0035 in/inDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inDry; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  55.0 MPa
@Temperature 160 °C
7980 psi
@Temperature 320 °F
ISO 527-1/-2
 60.0 MPa
@Temperature 140 °C
8700 psi
@Temperature 284 °F
ISO 527-1/-2
 70.0 MPa
@Temperature 120 °C
10200 psi
@Temperature 248 °F
Dry; ISO 527-1/-2
 85.0 MPa
@Temperature 100 °C
12300 psi
@Temperature 212 °F
Dry; ISO 527-1/-2
 110 MPa
@Temperature 80.0 °C
16000 psi
@Temperature 176 °F
Dry; ISO 527-1/-2
 145 MPa
@Temperature 23.0 °C
21000 psi
@Temperature 73.4 °F
Cond; ISO 527-1/-2
 155 MPa
@Temperature 23.0 °C
22500 psi
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 180 MPa
@Temperature -40.0 °C
26100 psi
@Temperature -40.0 °F
Dry; ISO 527-1/-2
Elongation at Break  2.3 %
@Temperature 23.0 °C
2.3 %
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 2.4 %
@Temperature 23.0 °C
2.4 %
@Temperature 73.4 °F
Cond; ISO 527-1/-2
 2.4 %
@Temperature -40.0 °C
2.4 %
@Temperature -40.0 °F
Dry; ISO 527-1/-2
 2.8 %
@Temperature 80.0 °C
2.8 %
@Temperature 176 °F
Dry; ISO 527-1/-2
 3.8 %
@Temperature 100 °C
3.8 %
@Temperature 212 °F
Dry; ISO 527-1/-2
 4.5 %
@Temperature 120 °C
4.5 %
@Temperature 248 °F
Dry; ISO 527-1/-2
 4.5 %
@Temperature 140 °C
4.5 %
@Temperature 284 °F
ISO 527-1/-2
 4.5 %
@Temperature 160 °C
4.5 %
@Temperature 320 °F
ISO 527-1/-2
Tensile Modulus  4.20 GPa
@Temperature 160 °C
609 ksi
@Temperature 320 °F
Dry; ISO 527-1/-2
 4.70 GPa
@Temperature 140 °C
682 ksi
@Temperature 284 °F
Dry; ISO 527-1/-2
 5.50 GPa
@Temperature 120 °C
798 ksi
@Temperature 248 °F
Dry; ISO 527-1/-2
 7.00 GPa
@Temperature 100 °C
1020 ksi
@Temperature 212 °F
Dry; ISO 527-1/-2
 9.00 GPa
@Temperature 80.0 °C
1310 ksi
@Temperature 176 °F
Dry; ISO 527-1/-2
 11.0 GPa
@Temperature 23.0 °C
1600 ksi
@Temperature 73.4 °F
Cond; ISO 527-1/-2
 11.5 GPa
@Temperature 23.0 °C
1670 ksi
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 12.0 GPa
@Temperature -40.0 °C
1740 ksi
@Temperature -40.0 °F
Dry; ISO 527-1/-2
Flexural Strength 230 MPa33400 psiDry; ISO 178
Flexural Modulus 10.0 GPa1450 ksiDry; ISO 178
Charpy Impact Unnotched 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Cond; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDry; IEC 60093
 >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmCond; IEC 60093
Dielectric Constant  3.7
@Frequency 1e+9 Hz
3.7
@Frequency 1e+9 Hz
Dry; IEC 60250
 3.9
@Frequency 1e+10 Hz
3.9
@Frequency 1e+10 Hz
Cond; IEC 60250
Dielectric Strength 33.0 kV/mm838 kV/inDry; IEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FDry; ISO 11359-1/-2
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°Fdry; ISO 11359-1/-2
Melting Point 325 °C617 °F10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 275 °C527 °FDry; ISO 75-1/-2
UL RTI, Electrical 150 °C
@Thickness 0.750 mm
302 °F
@Thickness 0.0295 in
UL746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM7905 / 291341

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.