Celanex 3409HR is a non-lubricated, 40% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability. To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250°F (121°C) for 4 hours. For subsequent storage of the material in the dryer until processed (<= 60 h) it is necessary to lower the temperature to 100° C.Information provided by Celanese Corporation. |
40% glass reinforced, hydrolytically stable, unlubricated |