MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Nylon 66, MoS2 Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, MoS2 Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.08 - 1.45 g/cc0.0390 - 0.0524 lb/in³Average value: 1.18 g/cc Grade Count:69
Water Absorption 0.900 - 8.50 %0.900 - 8.50 %Average value: 2.16 % Grade Count:20
Moisture Absorption at Equilibrium 0.400 - 8.50 %0.400 - 8.50 %Average value: 2.92 % Grade Count:8
Water Absorption at Saturation 7.00 - 8.50 %7.00 - 8.50 %Average value: 8.08 % Grade Count:6
Linear Mold Shrinkage 0.00200 - 0.0250 cm/cm0.00200 - 0.0250 in/inAverage value: 0.0129 cm/cm Grade Count:51
Linear Mold Shrinkage, Transverse 0.00300 - 0.0200 cm/cm0.00300 - 0.0200 in/inAverage value: 0.0140 cm/cm Grade Count:10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 84.0 - 88.084.0 - 88.0Average value: 85.5 Grade Count:4
Hardness, Rockwell R 100 - 120100 - 120Average value: 116 Grade Count:23
Hardness, Shore D 80.0 - 85.080.0 - 85.0Average value: 82.7 Grade Count:3
Tensile Strength, Ultimate 30.0 - 180 MPa4350 - 26100 psiAverage value: 84.5 MPa Grade Count:53
Tensile Strength, Yield 46.0 - 145 MPa6670 - 21000 psiAverage value: 86.9 MPa Grade Count:27
Elongation at Break 1.30 - 125 %1.30 - 125 %Average value: 21.9 % Grade Count:57
Elongation at Yield 3.50 - 100 %3.50 - 100 %Average value: 21.0 % Grade Count:9
Modulus of Elasticity 1.40 - 9.80 GPa203 - 1420 ksiAverage value: 3.57 GPa Grade Count:32
Flexural Yield Strength 11.7 - 265 MPa1700 - 38400 psiAverage value: 115 MPa Grade Count:61
Flexural Modulus 1.03 - 10.3 GPa149 - 1490 ksiAverage value: 3.40 GPa Grade Count:64
Compressive Yield Strength 8.27 - 110 MPa1200 - 16000 psiAverage value: 69.2 MPa Grade Count:5
Shear Strength 72.0 - 72.4 MPa10400 - 10500 psiAverage value: 72.3 MPa Grade Count:3
Izod Impact, Notched 0.270 - 7.88 J/cm0.506 - 14.8 ft-lb/inAverage value: 0.839 J/cm Grade Count:49
Izod Impact, Unnotched 0.587 - 5340 J/cm1.10 - 10000 ft-lb/inAverage value: 9.76 J/cm Grade Count:16
Izod Impact, Notched (ISO) 4.50 - 25.2 kJ/m²2.14 - 12.0 ft-lb/in²Average value: 11.2 kJ/m² Grade Count:9
 5.00 - 5.00 kJ/m²
@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 5.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 35.7 - 21000 kJ/m²17.0 - 9990 ft-lb/in²Average value: 35.7 kJ/m² Grade Count:3
 NB - NB
@Temperature -30.0 - -30.0 °C
NB - NB
@Temperature -22.0 - -22.0 °F
Grade Count:1
Charpy Impact Unnotched 2.00 - 2100 J/cm²9.52 - 9990 ft-lb/in²Average value: 52.0 J/cm² Grade Count:10
 5.00 - 6.50 J/cm²
@Temperature -40.0 - -40.0 °C
23.8 - 30.9 ft-lb/in²
@Temperature -40.0 - -40.0 °F
Average value: 6.00 J/cm² Grade Count:3
Charpy Impact, Notched 0.200 - 2.52 J/cm²0.952 - 12.0 ft-lb/in²Average value: 0.939 J/cm² Grade Count:18
 0.400 - 0.700 J/cm²
@Temperature -40.0 - -40.0 °C
1.90 - 3.33 ft-lb/in²
@Temperature -40.0 - -40.0 °F
Average value: 0.500 J/cm² Grade Count:3
Coefficient of Friction 0.230 - 0.2700.230 - 0.270Average value: 0.250 Grade Count:3
K (wear) Factor 70.0 - 383 x 10-8 mm³/N-M34.7 - 190 x 10-10 in³-min/ft-lb-hrAverage value: 252 x 10-8 mm³/N-M Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cm1.00e+12 - 1.00e+16 ohm-cmAverage value: 2.37e+15 ohm-cm Grade Count:23
Surface Resistance 1.00e+12 - 1.00e+14 ohm1.00e+12 - 1.00e+14 ohmAverage value: 4.90e+13 ohm Grade Count:9
Dielectric Constant 2.50 - 3.802.50 - 3.80Average value: 3.53 Grade Count:7
Dielectric Strength 11.8 - 120 kV/mm300 - 3050 kV/inAverage value: 35.5 kV/mm Grade Count:10
Dissipation Factor 0.0150 - 0.02000.0150 - 0.0200Average value: 0.0175 Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 64.8 - 90.0 µm/m-°C36.0 - 50.0 µin/in-°FAverage value: 75.2 µm/m-°C Grade Count:8
Thermal Conductivity 0.230 - 0.290 W/m-K1.60 - 2.01 BTU-in/hr-ft²-°FAverage value: 0.253 W/m-K Grade Count:6
Melting Point 249 - 275 °C480 - 527 °FAverage value: 259 °C Grade Count:26
Maximum Service Temperature, Air 79.4 - 200 °C175 - 392 °FAverage value: 129 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 180 - 254 °C356 - 490 °FAverage value: 225 °C Grade Count:35
Deflection Temperature at 1.8 MPa (264 psi) 64.0 - 250 °C147 - 482 °FAverage value: 101 °C Grade Count:59
Vicat Softening Point 240 - 255 °C464 - 491 °FAverage value: 245 °C Grade Count:6
Flammability, UL94 HB - V-2HB - V-2Grade Count:30
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 - 300 °C482 - 572 °FAverage value: 278 °C Grade Count:16
Melt Temperature 260 - 316 °C500 - 600 °FAverage value: 282 °C Grade Count:34
Mold Temperature 37.8 - 120 °C100 - 248 °FAverage value: 80.0 °C Grade Count:47
Drying Temperature 73.9 - 100 °C165 - 212 °FAverage value: 80.4 °C Grade Count:36
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.185 % Grade Count:11
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:8
Injection Pressure 4.96 - 124 MPa720 - 18000 psiAverage value: 65.3 MPa Grade Count:17
Vent Depth 0.000762 - 0.00127 cm0.000300 - 0.000500 inAverage value: 0.000889 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 66, Impact Grade
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
Overview of materials for Nylon 66, Extruded
Overview of materials for Nylon 66, PTFE Filled

O2509 / 78008

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.